Superalloys

Superalloys have a wide variety of applications, especially as the parts of gas turbines for aircraft and electric power stations. This book presents the results of the scientific studies on the three types of superalloys (Ni3Al-based, Iron-based, and Co3(Al,W)-based) including industrial gas turbine blades after accident.